This integrated technology addresses the challenges of high slime content, complex lithium mineral phases, and poor low-temperature adaptability of conventional reagents in hard-rock lithium ores.
Core components:
Lithium flotation collectors BK452 / BK429
Dense media separation (DMS) for pre-concentration and waste rejection
Pre-desliming & dephosphorization
Selective lithium flotation
Key outcomes:
Enables efficient recovery of multiple lithium minerals: spodumene, petalite, amblygonite, lepidolite
Improves lithium flotation recovery by 5–10%
Boosts associated Ta/Nb/Sn recovery by 10–30%
Reduces reagent consumption by 20–30%
Lowers impurity content in lithium concentrate; shortens Ta/Nb/Sn recovery flowsheet; cuts reagent dosage in winter operations
Proven in industrial application:Achieved stepwise recovery of petalite and spodumene, and significantly reducing phosphorus content in spodumene concentrate via simultaneous pre-separation of phosphorus and mica followed by selective lithium flotation. Targeted Complex lithium polymetallic resource development.